Professional-grade, two-part powder and binder system for precious metal casting. Designed for platinum, palladium, gold, silver, brass, copper, and similar metals.
Product Manual
Safety Data Sheet
| Name | Size | Quantity Per Pallet | Max Temp | Application |
|---|---|---|---|---|
| Ransom & Randolph | ||||
| Ultra-Vest |
48
24
|
1400°F (760°C) | Gold, Silver, Brass, Bronze | |
| Ultra-Vest Bandust |
48
|
1400°F (760°C) | Gold, Silver, Brass, Bronze, Low Dust Formula | |
| Ultra-Vest Maxx |
48
24
|
1450°F (788°C) | 18kt White Gold | |
| Plasticast |
48
|
1400°F (760°C) | CadCam Resin & Thermo-Plastic Waxes | |
| Plasticast Bandust |
48
|
1400°F (760°C) | CadCam Resin & Thermo-Plastic Waxes Low Dust Formula | |
| SC20 Satin Cast |
24
|
1350°F (730°C) | Gold, Silver, Brass, Bronze | |
| SC-X Satin Cast Xtreme |
24
|
1450°F (788°C) | 18kt White Gold | |
| Liberty-Vest |
48
|
1350°F (730°C) | Wax & Resin Casting | |
| Solitaire |
48
|
1166°F (630°C) | Stone in Wax Casting | |
| Astro-Vest |
48
|
2200°F (1200°C) | High Temp Alloys No Binder Required | |
| Blue Label Platinum Investment w/ Binder |
24
|
1600°F (871°C) | High Temp Alloys w/ Platinum Binder | |
| Plasti-Cast PT w/ Phosphate Binder |
48
|
1600°F (871°C) | Designed for high-temperature alloy casting, ideal for plastic and wax/plastic pattern materials | |
| Yasui | ||||
| HI-Temp Fuji Powder w/ Binder |
24
|
1650°F (898°C) | Platinum & Hi-Temp Alloys 2-Part Investment | |
| Romanoff | ||||
| J-Formula Platinum Investment w/ White Binder |
48
|
1600°F (871°C) | Platinum & Hi-Temp Alloys 2-Part Investment | |
| J-Formula Platinum Investment w/ Orange Binder |
48
|
1600°F (871°C) | Platinum & Hi-Temp Alloys 2-Part Investment | |
| J-Formula Platinum Investment Orange Label Powder Only |
48
|
1600°F (871°C) | Platinum & Hi-Temp Alloys 2-Part Investment Powder Only | |
| J-Formula Platinum Investment w/ Blue Binder |
48
|
1600°F (871°C) | Platinum & Hi-Temp Alloys 2-Part Investment | |
Doc's is designed for fast and flexible metal casting, supporting a range of metals such as platinum, palladium gold, silver, brass, and copper.
It enables jewelers to complete the casting process from wax to finished piece in under four hours, with a rapid burn-out time of just 2½ hours—ideal for quick, small-batch production. The investment material sets quickly, requires mixing for preparation, and produces a smooth surface finish.
Note: Flaskless casting is ideal with this type of material.
Country of Origin: United States
Style: Doc's Casting Plaster
Weight: 25 lbs (11.4 kg)
Application: Platinum, Palladium, Gold, Silver, Brass, Copper & Alternative Metals
Max Oven Temperature: 1700°F (927°C)
Manufacturer: Ransom & Randolph