Ransom & Randolph Plasticast PT Investment & Liquid Binder 44 lbs

SKU:Z14-304-PT44

Regular price $377.50
$377.50
Sale price
Regular price
Sale Sold out

Plasticast® PT Investment & Binder System is designed for investing and burnout of commonly used plastic and wax/plastic patterns up to 1600°F (871°C). Its high expansion and extra-high strength help accommodate the demands of these pattern materials during burnout while maintaining mold integrity. The system delivers reliable performance, smooth surface quality, and dimensional accuracy for high-temperature metal casting.



  • American Express
  • Apple Pay
  • Bancontact
  • Diners Club
  • Discover
  • Google Pay
  • Mastercard
  • Shop Pay
  • Visa




Name Size Quantity Per Pallet Max Temp Application
Ransom & Randolph
Doc's Casting Plaster
44
1700°F (871°C) Fast 2 ½ hour burnout cycles
Great for all Low & High Temp Metals
Ultra-Vest
48
24
1400°F (760°C) Gold, Silver, Brass, Bronze
Ultra-Vest Bandust
48
1400°F (760°C) Gold, Silver, Brass, Bronze, Low Dust Formula
Ultra-Vest Maxx
48
24
1450°F (788°C) 18kt White Gold
Plasticast
48
1400°F (760°C) CadCam Resin & Thermo-Plastic Waxes
Plasticast Bandust
48
1400°F (760°C) CadCam Resin & Thermo-Plastic Waxes Low Dust Formula
SC20 Satin Cast
24
1350°F (730°C) Gold, Silver, Brass, Bronze
SC-X Satin Cast Xtreme
24
1450°F (788°C) 18kt White Gold
Liberty-Vest
48
1350°F (730°C) Wax & Resin Casting
Solitaire
48
1166°F (630°C) Stone in Wax Casting
Astro-Vest
48
2200°F (1200°C) High Temp Alloys No Binder Required
Blue Label Platinum Investment w/ Binder
24
1600°F (871°C) High Temp Alloys w/ Platinum Binder
Plasti-Cast PT w/ Phosphate Binder
48
1600°F (871°C) Designed for high-temperature alloy casting, ideal for plastic and wax/plastic pattern materials
Yasui
HI-Temp Fuji Powder w/ Binder
24
1650°F (898°C) Platinum & Hi-Temp Alloys 2-Part Investment
Romanoff
J-Formula Platinum Investment w/ White Binder
48
1600°F (871°C) Platinum & Hi-Temp Alloys 2-Part Investment
J-Formula Platinum Investment w/ Orange Binder
48
1600°F (871°C) Platinum & Hi-Temp Alloys 2-Part Investment
J-Formula Platinum Investment Orange Label Powder Only
48
1600°F (871°C) Platinum & Hi-Temp Alloys 2-Part Investment Powder Only
J-Formula Platinum Investment w/ Blue Binder
48
1600°F (871°C) Platinum & Hi-Temp Alloys 2-Part Investment

Country of Origin: United States

Style: Plasti-Cast PT w/ Phosphate Binder

Weight: 44 lbs (20.0 kg)

Application: Designed for high-temperature alloy casting, ideal for plastic and wax/plastic pattern materials

Max Oven Temperature: 1600°F (871°C)

Manufacturer: Ransom & Randolph